FXBW-04 Acrylic Acid Modified Polysiloxane Finish
[Search Related Products]
FXBW-04 Acrylic Acid Modified Polysiloxane Finish (different colors) (use for steel structures)
Characteristics: excellent elements resistance¡¢resistance of ultraviolet radiation irradiation property¡¢excellent resistance of acid¡¢alkali¡¢oil¡¢water and antifouling property¡¢good gloss and color retention and high gloss decorative (gloss and color retention is the acrylic acid polyurethane paint more than 4 times)¡¢innoxious¡¢environmental protection.
Uses: mainly use for bridge¡¢stadiums¡¢conference and exhibition center¡¢airport¡¢petrochemical plant etc. steel structure anticorrosion.
Technical target£º
Mixing ratio: Host crystal/Firming agent=100/8(by weight)
Standard film thickness: Dry: 30¦Ìm/coat
Academic spreading rate: 0.07kg/ ©O/30¦Ìm
Solid contents: 70%
Humidity requirement: below 85%
Drying time & Coating interval
Temperature £¨¡æ£© |
10 |
02 |
30 |
Dry to touch£¨hrs£© |
60 |
50 |
25 |
Dry semi-hard£¨hrs£© |
12 |
8 |
6 |
Min. interval£¨hrs£© |
24 |
12 |
8 |
Substrate treatment£ºPrimer surface must thoroughly clean¡¢dry¡¢no dew
Matching£º
Applicable under coatings: Epoxy primers¡¢epoxy intermediate paint
Application of FXBW-04 Acrylic Acid Modified Polysiloxane Finish: